In this post, i will review a journal from Muhammad A.Butt, Muhammad A.Virk, Arshad Chungtai, Ijaz H.Khan, Munir Ahmad. They are from Institute of Chemical Engineering and Technology, university of Punjab, New Campus Lahore, Pakistan and Technical Services Centre, Pakistan Standard and Quality Control Authority, 125 A Industrial Area, Kot Lakhpat, Lahire, Pakistan. The title is "T-Type Naphta Pump Strainer Mesh Failure Analysis".
Here it is!
Note: This post is related with one of my subject namely advanced corrosion
Stress Corrosion Cracking- T Type Naphta Pump Strainer Mesh Failure Analysis